Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 685.0 - 771 °C | 1265 - 1420 °F | |
Lucas-Milhaupt Silvaloy® A25T Brazing Alloy Silvaloy A25T is an economical filler metal for ferrous and nonferrous joints not requiring high ductility or impact strength. It is similar to Silvaloy A40T, however flow is less active and tempera.. |