Thermal Properties Metric English Comments
Melting Point 743 - 760 °C
1370 - 1400 °F
Williams Advanced Alloys Wambraze™ WB760 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..