Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 338 - 390 °C | 640 - 734 °F | |
Johnson Matthey LM 5 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |