Polymer Property : Melting Point = 72.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 72.2 °C
162 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil ESCOR™ AT 320 Blown Film Resin  (discontinued **)
ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical
Melting Point 72.2 °C
162 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil ESCOR™ AT 320 Cast Film Resin  (discontinued **)
ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical
Melting Point 72.2 °C
162 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil EXACT™ 4056 Plastomer for Film Blends and Blown Film Applications
Product Description: Exact 4056 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin can be used in blends with polyolefins to improve..
Melting Point 72.2 °C
162 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate
OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low ..
Melting Point 72.2 °C
162 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil OPTEMA™ TC 220 ExCo Ethylene Methyl Acrylate
Product Description: Product Description: Optema TC 220 is an ethylene methyl acrylate copolymer, which can be used for making alloys, blends and compounds or be injection molded where softness and ..
Melting Point 72.2 - 102 °C
162 - 216 °F
Average value: 87.9 °C Grade Count:17
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an..
Copyright © lookpolymers.com All Rights Reserved