Thermal Properties Metric English Comments
Melting Point 657.2 - 688 °C
1215 - 1270 °F
Lucas-Milhaupt FOS FLO 670 Copper Phosphorus Tin Braze Filler Metal
Applications:Fos-Flo 7 iFos-Flo 670 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encounter..
Melting Point 646.1 - 688 °C
1195 - 1270 °F
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy
Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu..
Melting Point 632 - 688 °C
1170 - 1270 °F
Lucas-Milhaupt EASY FLO 3 Carbide Brazing Alloy
Easy-Flo 3 is recommended for use on stainless steels subject to chloride corrosion, such as marine hardware, fishing tackle, and some dairy equipment cleaned with bleaching solutions and other equi..
Melting Point 632 - 688 °C
1170 - 1270 °F
Lucas-Milhaupt Silvaloy® 50N Brazing Alloy
Silvaloy 50N is a modification of Silvaloy 50. It was originally introduced because of somewhat better corrosion resistance than Silvaloy 50 for certain conditions, and is still used for such purpos..
Melting Point 632 - 688 °C
1170 - 1270 °F
Universal Wire Works BAg-3 (AMS 4771) Silver Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.