Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 680 - 705 °C | 1260 - 1300 °F | |
Johnson Matthey Argo-braze 49H Silver Brazing Alloy for Tungsten Carbide Brazing Optimum Joint Gap 0.1 - 0.25 mm.AWS A5.8-92 BAg-22BS EN 1044 1999 AG502Equivalent to Engelhard Silvaloy A-49NMEquivalent to Handy & Harman Braze 495Information provided by Johnson Matthey. |