Polymer Property : Melting Point = 638 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point >= 337 °C
>= 638 °F
Customer Specified
Heatbath/Park Aluminum Casting Salt AC Aluminum Casting Salt
Salt cores can be made with varying melting points to meet the needs of customers who gravity cast as well as those using state-of-the-art die casting machines. Advantages of salt cores over sand c..