Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 621 °C | 1150 °F | |
Parkway Products Thixomolded® AM50A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Melting Point | 621 °C | 1150 °F | |
MarkeTech Cesium Iodide:Thallium (CsI:Tl) Scintillator Crystal Cesium Iodide activated by thallium is a scintillation material with high absorption power and can be used as an efficient gamma ray absorber. CsI:Tl is soluble in water, but is not hygroscopic in l.. |
|||
Melting Point | 621 °C | 1150 °F | |
Mateck Cesium Iodide, CsI Optical crystals |