Thermal Properties Metric English Comments
Melting Point 16.0 - 25.0 °C
60.8 - 77.0 °F
Indium Corp. Indalloy 77 Fusible Gallium Alloy
Information Provided by Indium Corporation
Melting Point 16.0 °C
60.8 °F
Eutectic
Indium Corp. Indalloy® 60 Ga-In Eutectic Alloy for Mercury Replacement
Alloy liquid at room temperature, wets glass and quartz. Mercury replacement.Information provided by the manufacturer, Indium Corporation.