Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 13.0 - 14.0 °C | 55.4 - 57.2 °F | |
BASF N-Vinyl-2-pyrrolidone, Non-Stabilized Formula: C6H9NOCAS: 88-12-0Description: Vinyl pyrrolidone is a colorless to yellowish liquid, with a characteristic odor. It is miscible in water and organic solvents.Synonyms: N-Vinylpyrrolidone, .. |
|||
Melting Point | 12.0 - 14.0 °C | 53.6 - 57.2 °F | |
BorsodChem ONGRONAT T 80 TDI 80/20 Isocyanate Description of product:Appearance: At room temperature water clear liquid. Composition: A mixture of toluene-di-isocyanate isomers (2,4-toluene-di-isocyanate [A] and 2,6-toluene-di-isocyanate [B].No.. |