Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 55.6 °C | 132 °F | |
ChevronTexaco 128 Refined Wax FeaturesChevron Refined Waxes are fully refined, food grade waxes meeting the highest purity standards. Derived from petroleum using a solvent refining process, Chevron Refined Waxes are comprised .. |