Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 3017 °C | 5463 °F | |
H.C. Starck NRC® Tantalum (UNS R05200) Applications: High strength and excellent corrosion resistance make tantalum ideal for use in the manufacture and repair of chemical process equipment and heat exchangers. Other uses are rupture di.. |