Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 284 °C | 543 °F | DSC |
Ensinger Tecatron® XP-64B Compression Molded PPS Compound, 40% Fiberglass, Black Pigmented Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |