Thermal Properties Metric English Comments
Melting Point 11.0 - 17.0 °C
51.8 - 62.6 °F
Indium Corp. Indalloy® 51 Ga-In-Sn Alloy for Mercury Replacement
Alloy liquid at room temperature, wets glass and quartz. Mercury replacement.Information provided by the manufacturer, Indium Corporation.
Melting Point 11.0 °C
51.8 °F
Eutectic
Indium Corp. Indalloy 51E Low Melting Gallium Alloy
Information Provided by Indium Corporation
Melting Point 11.0 °C
51.8 °F
BASF 3-Amino-1-propanol
Formula: C3H9NOCAS: 156-87-6Description: 3-amino-1-propanol is a colorless to yellow liquid with an amine-like odor. It is miscible with water in all proportions. Synonyms: Propanolamine, 3-aminopr..