Thermal Properties Metric English Comments
Melting Point 2758 °C
4996 °F
Zircar Zirconia HfF-100 Hafnia Felt Insulation
Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are off..
Melting Point 2758 °C
4996 °F
Zircar Zirconia HfF-15 Hafnia Knit Textile Insulation
Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are off..
Melting Point 2758 °C
4996 °F
Zircar Zirconia HfF-100 Hafnia Felt Insulation
Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are off..
Melting Point 2758 °C
4996 °F
Zircar Zirconia HfF-15 Hafnia Knit Textile Insulation
Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are off..