Thermal Properties Metric English Comments
Melting Point 41.0 °C
106 °F
Peak; ExxonMobil Method
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin
Product Description: Exact 9061 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Melting Point 41.0 °C
106 °F
Peak; ExxonMobil Method
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin
Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Melting Point 41.0 °C
106 °F
BASF Hexamethylenediamine
Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical synthesesInformation provided by BASF