Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 193.3 °C | 379.9 °F | ISO 11357-2 |
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing Processed by selective laser sintering (SLS). Windform® SP is a deep black composite polyamide that is a “Top” level material within the polyamide Windform® materials for additive manufacturing.. |