Polymer Property : Melting Point = 375.3 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 190.7 °C
375.3 °F
ASTM D3418
CRP Technology Windform® FX Polyamide Composite
Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive..