Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2053 °C | 3727 °F | |
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip ZIRCAR hanger clips are comprised of sapphire (single crystal aluminum oxide) and are designed for use with hanger rod (HR-1). The single crystal structure of these clips prevents creep and deformat.. |