Polymer Property : Melting Point = 356.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 180.0 °C
356.0 °F
ASTM D3418
CRP Technology Windform® LX 2.0 Polyamide Composite
Processed by selective laser sintering (SLS). Windform® LX 2.0 has improved the already excellent performances of Windform® LX and this can be noticed from technical properties and sinterability ..