Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 179.3 °C | 354.7 °F | ISO 11357-2 |
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its.. |
|||
Melting Point | 179.3 °C | 354.7 °F | ASTM D3418 |
CRP Technology Windform® XT Polyamide-Carbon Composite WindForm™ XT Composite is a new generation material, in which the mechanical characteristics are excellent for Rapid Manufacturing. Black coloured compound polyamide and carbon based material with .. |