Thermal Properties Metric English Comments
Melting Point 1830 - 1855 °C
3330 - 3371 °F
Goodfellow Platinum 90/Rhodium 10 Thermocouple Alloy
The positive element of the type S thermocouple. Type S thermocouples are characterized by a high degree of chemical inertness and stability at high temperatures. Often used as a standard for calibr..