Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 328 - 334 °C | 622 - 633 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Algoflon® L206 Polytetrafluoroethylene (PTFE)
(Unverified Data**) Algoflon® L206 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It is specially recommended for use as an additive in elastomers (e.g. perfluoroelastomers) t.. |