Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | <= 1.00 °C | <= 33.8 °F | Freezing Point |
Solvay TOLCIDE® PS 20A 20% tetrakis hydroxymethyl phosphonium sulfate Identification: Proprietary formulation based upon TETRAKIS (HYDROXYMETHYL) PHOSPHONIUM SULPHATE (THPS CAS NR 55566-30-8) and a biopenetrantAvailable in: North AmericaFoam potential: Non-foamingFunc.. |
|||
Melting Point | 1.00 - 10.0 °C | 33.8 - 50.0 °F | |
BASF Sarcosine Sodium 40% Solution Formula: C3H6NNaO2CAS: 4316-73-8Description: Sarcosine Sodium 40% sol. is a colorless to yellowish liquid, with no odor. It is miscible with water in all proportions.Synonyms: N-Methylglycine monos.. |