Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1705 °C | 3101 °F | |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Melting Point | <= 1705 °C | <= 3101 °F | |
TIMET TIMETAL® 6-2-4-2 (Ti-6Al-2Sn-4Zr-2Mo-0.08Si) Titanium Alloy Medium-Strength, Elevated Temperature AlloyIndustry Specifications: USA Aerospace: AMS 4919.Features: TIMETAL 6-2-4-2 has good tensile creep and fatigue properties up to 540°C. It is the most comm.. |