Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 143 - 154 °C | 290 - 310 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |