Polymer Property : Melting Point = 285 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 141 - 145 °C
285 - 293 °F
ASTM D3418
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..