Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1530 °C | 2790 °F | |
Goodfellow Nickel 79/Aluminum 21 Alloy Information provided by Goodfellow. |
|||
Melting Point | <= 1530 °C | <= 2790 °F | |
CMW® D57F Silver Iron Contact Material For electrical contacts; AC resistive loads.Information provided by CMW Inc. |