Polymer Property : Melting Point = 272.3 °F
Polymer Property :
Melting Point =
272.3 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Melting Point
133.5
°C
272.3
°F
ASTM D3418
Arkema Group Pebax® 2533 Polyether Block Amide (PEBA)