Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 269 °C | 516 °F | DSC |
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge Teonex® Q51 is biaxially oriented polyethylene naphthalate (PEN) film. It is slightly hazy with excellent handling properties for general purpose. It is commercially available in nominal 48 - 1000 .. |
|||
Melting Point | 269 °C | 516 °F | DSC |
DuPont Teijin Films Teonex® Q72 Polyester Film, 14 Gauge Teonex® Q72 is biaxially oriented, slightly hazy polyethylene naphthalate (PEN) film. This ultra thin film which was developed for capacitor applications. It is commercially available in nominal 14.. |
|||
Melting Point | 269 °C | 516 °F | DSC |
DuPont Teijin Films Teonex® Q83 Polyester Film, 200 Gauge Teonex® Q83 is biaxially oriented, slightly hazy polyethylene naphthalate (PEN) film with excellent handling properties and high dimensional stability. It is commercially available in 100, 200 and .. |