Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 263.0 °C | 505.4 °F | ISO 3146-C |
Solvay Technyl® A216V15 15% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melting Point | 263.0 °C | 505.4 °F | ISO 3146-C |
Solvay Technyl® A218V43 43% Glass Filled, Heat Stabilized Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melting Point | 263.0 °C | 505.4 °F | ISO 3146-C |
Solvay Technyl® A238 Unfilled, Heat Stabilized, Impact Modified Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melting Point | 263.0 °C | 505.4 °F | |
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |