Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 126.3 °C | 259.3 °F | ASTM D3418 |
LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade Alathon H4620 is a medium-flow resin that exhibits good cold temperature impact performance, enhanced processing and thermal stability. Typical applications are thinner-walled parts that require che.. |