Melting Point 1414 °C
2577 °F
American Elements Silicon Nanoparticles
General DescriptionSilicon (Si) Nanoparticles, nanodots or Nanopowder are spherical high surface area metal particles. Nanoscale Silicon Particles are typically 5-25 nanometers (nm) with specific su..
Melting Point 1414 °C
2577 °F
American Elements Silicon Nanotubes
General DescriptionSilicon (Si) Nanotubes, Single-Walled, Double Walled and Multi-Walled are tubular ultra high surface area nanotubes. Nanoscale Silicon Nanotubes are typically 10 - 100 nanometers ..