Melting Point 1338 - 1366 °C
2440 - 2491 °F
Kennametal Stellite Stellite® 21
Excellent high temperature strength, high toughness. Solution treat at 1191-1204°C, rapid air cool, age between 538-871°C to increase hardness and strength at the expense of impact and ducti..
Melting Point 1311 - 1366 °C
2392 - 2491 °F
Special Metals INCOLOY® Alloy 925
A precipitation-hardenable nickel-iron-chromium alloy with additions of molybdenum and copper. It combines the high strength of a precipitation-hardenable alloy with the excellent corrosion resista..