Polymer Property : Melting Point = 2482 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1332 - 1361 °C
2430 - 2482 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Melting Point 1332 - 1361 °C
2430 - 2482 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Melting Point 1332 - 1361 °C
2430 - 2482 °F
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Melting Point 1332 - 1361 °C
2430 - 2482 °F
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Melting Point 1332 - 1361 °C
2430 - 2482 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..