Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1196 - 1330 °C | 2185 - 2430 °F | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H925 (H925) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Melting Point | 1300 - 1330 °C | 2370 - 2430 °F | |
Special Metals UDIMET® alloy 188 Cobalt-base Alloy UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small .. |
|||
Melting Point | 1196 - 1330 °C | 2185 - 2430 °F | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Melting Point | 1196 - 1330 °C | 2185 - 2430 °F | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H1050 (H1050) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Melting Point | 1196 - 1330 °C | 2185 - 2430 °F | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H775 (H775) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |