Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1255 - 1308 °C | 2291 - 2386 °F | |
Kennametal Stellite Delcrome® 90 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. White cast iron, abrasion resistant. Carbide modifiers can provide a refined microstructure and.. |