Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2335 °C | 4235 °F | |
American Elements Samarium Oxide Nanopowder General DescriptionSM-MITE powders and dispersions are inorganic samarium-oxide nanoparticles. SM-MITE-A products are uncoated and hydrophilic. SM-MITE-O products are coated with an organic silane (.. |