Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2300 °C | 4170 °F | |
Specialty Materials Boron Monofilament Exceptional compression strength. Specialty Materials' Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source.Information prov.. |
|||
Melting Point | 2300 - 2400 °C | 4170 - 4350 °F | |
ATI Wah Chang Nb/Nb Alloy C-103 This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig.. |