Polymer Property : Melting Point = 219.47 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 219.47 °C
427.05 °F
Nylacast Impact Nylon 6, Impact Grade
Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also..