Melting Point 1070 - 1160 °C
1960 - 2120 °F
Kennametal Stellite Deloro® 22 Nickel Alloy
Deloroâ„¢ 22 is a pre-alloyed gas atomized nickel based powder which is used primarily for the local repair and hardfacing of glass forming molds. It can also be used as a tough build-up alloy fo..