Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2080 °C | 3780 °F | |
MarkeTech Strontium Titanate (SrTiO3) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
Melting Point | 2080 °C | 3780 °F | |
MarkeTech Thorium-Doped Lanthanum Aluminum Oxide (Th:LaAlO3) Single Crystal Substrate Data provided by MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
Melting Point | 2080 °C | 3780 °F | |
Mateck Nb:SrTiO3 Substrate bicrystals for superconductivity |
|||
Melting Point | 2080 °C | 3780 °F | |
Mateck SrTiO3 Substrate bicrystals for superconductivity |
|||
Melting Point | 2080 °C | 3780 °F | |
Mateck Strontium Titanium Substrate, SrTiO3 Substrate single crystals for superconductivity |