Thermal Properties Metric English Comments
Melting Point 1135 - 1169 °C
2075 - 2136 °F
Universal Wire Works BAu-5 (AMS 4785) Gold Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Melting Point 1135 - 1169 °C
2075 - 2136 °F
Williams Advanced Alloys Wambraze™ WB1169 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..