Polymer Property : Melting Point = 2050 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 2050 °C
3720 °F
Misumi Alumina 96 Aluminum Oxide, Al2O3
Information provided by MISUMI Corporation.
Melting Point 2050 °C
3720 °F
Goodfellow Ruby, Al2O3
Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro..
Melting Point 2050 °C
3720 °F
Zircar Refractory Composites Alumina Coat
ZRCI ALUMINA COAT is an all-alumina liquid formulation used for hardening and increasing the refractoriness of the surfaces of alumina and alumina-silicate fiber products. ZRCI ALUMINA COAT is comp..
Melting Point 2050 °C
3720 °F
Zircar Ceramics AL-R/H Alumina Rigidizer/Hardener
Type AL-R/H Alumina Rigidizer/Hardener is a single part water based colloidal suspension of alumina hydrate. Mainly used for rigidizing and hardening the surfaces of ZIRCAR® fibrous ceramic product..