Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1102 - 1120 °C | 2016 - 2050 °F | |
Universal Wire Works Au-Pd-Ni (AMS 4784) Gold Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Melting Point | 1102 - 1121 °C | 2016 - 2050 °F | |
Williams Advanced Alloys Wambraze™ WB1121 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |