Polymer Property : Melting Point = 2015 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 2015 °C
3659 °F
Zircar Zirconia ALF-100 Alumina Felt Insulation
Alumina (Al2 O3) has excellent thermal shock resistance, high dimensional stability and good chemical inertness, which makes our alumina fiber products ideal for fast firing cycles up to 1700°C. Ou..
Melting Point 2015 °C
3659 °F
Zircar Zirconia ALK-15 Alumina Knit Textile Insulation
Alumina (Al2 O3) has excellent thermal shock resistance, high dimensional stability and good chemical inertness, which makes our alumina fiber products ideal for fast firing cycles up to 1700°C. Ou..
Melting Point 2015 °C
3659 °F
Zircar Zirconia ALF-100 Alumina Felt Insulation
Alumina (Al2 O3) has excellent thermal shock resistance, high dimensional stability and good chemical inertness, which makes our alumina fiber products ideal for fast firing cycles up to 1700°C. Ou..
Melting Point 2015 °C
3659 °F
Zircar Zirconia ALK-15 Alumina Knit Textile Insulation
Alumina (Al2 O3) has excellent thermal shock resistance, high dimensional stability and good chemical inertness, which makes our alumina fiber products ideal for fast firing cycles up to 1700°C. Ou..