Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1435 - 2002 °C | 2615 - 3635 °F | |
Carlson C 200 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |