Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 980.0 - 1080 °C | 1796 - 1976 °F | |
Cadi 150 Copper Alloy A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electr.. |
|||
Melting Point | 980.0 - 1080 °C | 1796 - 1976 °F | |
Cadi 1815 Copper Alloy Zirconium addition to chromium copper improves creep resistance at high operating temperatures and reportedly reduces sticking of electrodes to the work during spot welding of galvanized materials. .. |
|||
Melting Point | 1070 - 1080 °C | 1958 - 1976 °F | |
Cadi 182 Copper Alloy Chromium copper is the primary copper alloy used for resistance spot and seam welding. This alloy achieves good hardness and electrical conductivity through a combination of heat treatment and cold .. |