Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1050 °C | 1920 °F | |
Reade Advanced Materials Ilmenite Powder (FeTiO3) Description: A naturally mined iron titanium oxide mineral. It is generally black as sand, odorless, tasteless, opaque under a microscope, non-flammable and insoluble at 20 deg. C. Physical Properti.. |
|||
Melting Point | 1050 °C | 1920 °F | |
MarkeTech BGO (Bismuth Germanate, Bi4Ge3O12) Scintillator Crystal Bismuth germanate is intrinsic scintillation material with high absorption power. Due to its high effective atomic number and high density, BGO is a very efficient gamma absorber with high photo eff.. |