Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1020 °C | 1868 °F | |
California Fine Wire Manganin 230 (Shunt) Copper, Manganese, and Nickel Resistance Wire All values may vary dependent on specific design and usageNickel content modifiedCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1020 °C | 1868 °F | |
California Fine Wire Manganin 290 Copper, Manganese, and Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |